Research of the main parameters of the technological process of electric contact welding at the restoration of machine parts

dc.contributor.authorDudnikov, A. A.
dc.contributor.authorDudnikov, I. A.
dc.contributor.authorDudnyk, V. V.
dc.contributor.authorGorbenko, O. V.
dc.contributor.authorKelemesh, A. O.
dc.contributor.authorДудніков, Анатолій Андрійович
dc.contributor.authorДудніков, Ігор Анатолійович
dc.contributor.authorДудник, Володимир Васильович
dc.contributor.authorГорбенко, Олександр Вікторович
dc.contributor.authorКелемеш, Антон Олександрович
dc.date.accessioned2018-03-30T11:00:03Z
dc.date.available2018-03-30T11:00:03Z
dc.date.issued2017-11
dc.description.abstractThe object of research is the process of restoring lancet cultivator paws by electrocontact welding of their working parts, the process connection with technological processing parameters and the physical and mechanical properties of their material. One of the most problematic places in the method of electrocontact welding when restoring the working organs of tillage machines is the lack of optimal operating parameters of this technological process of strengthening the cutting elements of working organs working in the soil-aggressive environment. Optimal parameters of electrocontact welding method of the metal mesh to the worn-out surface of the part make it possible to increase the strength of the material of the recovered parts, improve its physical and mechanical properties and increase their service life, and to reduce the magnitude and irregularity of wear. Theoretical studies of the main parameters of the technological process are carried out using the equations of mechanics of deformed bodies with their own physical and mechanical properties. In the course of the study, a steel mesh made of high-strength steel is used, and metal powders are used as a filler material, which strengthened the material of the component and increased its life. Increased wear resistance of the restored parts is obtained. This is due to the fact that with this technological process, the formation of the surface relief takes place with the formation of depressions on it, which retain the lubricant, which ensures a higher coating resistance. Due to this, it is possible to obtain a coating of parts with a thickness of up to 1.5 mm, an increase in their durability of 1.45–2.1 times and a decrease in wear intensity of 1.65 times compared to new cultivator paws.uk_UA
dc.identifier.citationDudnikov A., Dudnikov I., Dudnik V., Gorbenko O., Kelemesh A. Research of the main parameters of the technological process of electric contact welding at the restoration of machine parts//Technology audit and production reserves. 2017. 6/1(38). P.4-9.uk_UA
dc.identifier.issn2226-3780
dc.identifier.urihttps://dspace.pdau.edu.ua/handle/123456789/293
dc.language.isoenuk_UA
dc.publisherTechnology audit and production reserves, НВП ПП «Технологічний Центр»uk_UA
dc.relation.ispartofseriesIndustrial and technology systems: mechanical engineering technology;6/1(38)
dc.subjectelectrocontact weldinguk_UA
dc.subjecttechnological processuk_UA
dc.subjectabrasive wearuk_UA
dc.subjectadhesion strengthuk_UA
dc.subjectcoating propertiesuk_UA
dc.titleResearch of the main parameters of the technological process of electric contact welding at the restoration of machine partsuk_UA
dc.title.alternativeДослідження основних параметрів технологічного процесу електроконтактного приварювання при відновленні деталей машинuk_UA
dc.typeArticleuk_UA
Files
Original bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
Dudnikov, Dudnik, Gorbenko, Kelemesh (TARP_2017).pdf
Size:
898.36 KB
Format:
Adobe Portable Document Format
Description:
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: